I-LiNbO3 Crystal
LiNbO3 (I-Lithium Niobate) i-crystal yindawo yokusebenza ehlanganisa iipyzoelectric, i-Ferroelectric, pyroelectric, i-nonlinear, i-electro-optical, ifotoelastic, njl. Njl LiNbO3 inozinzo olufanelekileyo lwe-thermal kunye nokuqina kweekhemikhali.
Njengenye yezinto ezibonakalayo ezibonakalayo ezingalulanga ngamehlo ezi-nonlinear, i-LiNbO3 Ilungele iintlobo ezahlukeneyo zesicelo sokuguqula imijikelezo. Umzekelo, isetyenziswa ngokubanzi njengabaphindaphindi abaphindiweyo bexesha le-wavelength> I-1 μm kunye ne-oscillator yee-octillometri (ii-OPOs) zepumitha ngo-1064 nm kunye nezixhobo ze-quasi-phase-matched (QPM). Ngenxa ye-EO enkulu kunye ne-AO coefficients, iLiNbO3 I-Crystal isetyenziswa rhoqo kwiimodyuli zesigaba, i-waveguide substrate, umphezulu we-acoustic wave wafers, kunye ne-Q-switch of Nd: YAG, Nd: YLF kunye ne-Ti-Sapphire lasers.
LiNbO3 Unokufakwa kumachaphaza ngezinto ezahlukeneyo, ezinjenge-Er, Pr, Mg, Fe, njl. njl. Umzekelo, umqobo womqobo weMgO: LiNbO3 ingaphezulu kokuphindwe kabini kweLiNbO emsulwa3.
Nxibelelana nathi malunga nesisombululo esona sisicelo sakho seLiNbO3 amakristali.
Ubuchule be-WISOPTIC -LiNbO3
• Iindidi ezahlukeneyo zamacandelo agqityiweyo zicelo ezahlukeneyo.
• Ukulawulwa kwekhwalithi engqongqo
Ukuhanjiswa okuqinisekileyo
• Amaxabiso okhuphiswano kakhulu
• Uxhaso lobuchwepheshe
Ukucaciswa kweMigangatho yeWISOPTIC* -I-LiNbO3
Ukunyamezeleka konyamezelo | ± I-0,5 mm |
Ukunyamezelana kwengqondo | ± I-0.5 ° |
I-Flatness | <λ / 8 @ 632.8 nm |
Umgangatho ongaphezulu | <20/10 [S / D] |
Ukufana | <20 " |
Ukuzibophelela | ≤ 5 ' |
I-Chamfer | ≤ I-0mmmm @ ngu-45 ° |
Ukuhanjiswa kweLitye elandisiweyo | <λ / 4 @ 632.8 nm |
Ukucoca iapile | > 90% indawo ephakathi |
Ukupheka | Umdibaniso we-AR: R <0.2% @ 1064 nm, R <0.5% @ 532 nm |
* Iimveliso ezinemfuno ekhethekileyo xa uceliwe. |
Izibonelelo zeM MgO: I-LiNbO3 kuthelekiswa neLiNbO3
Efficiency Ukusebenza ngokuphezulu okuphindaphindiweyo okuphindwe kabini (SHG) kwimpundu Nd: YAG (65%) kunye neCW Nd: YAG (45%)
Ukusebenza okuphezulu kwizicelo ze-OPO, i-OPA, ii-QPM eziphindwe kabini kunye ne-waveguide edityanisiweyo
• Umqobo omkhulu womonakalo wefotorefractive
Izicelo eziPrayimari -iLiNbO3
Iiphindaphindwe eziphindaphindiweyo zamaza omda> 1 μm
• I-oscillator ye-Optical parametric oscillators (OPO) ifakwe kwi-1064 nm
Izixhobo ze-Quasi-phase-matched (QPM)
Ukutshintsha kwe-Q (kwe-Nd: YAG, Nd: YLF kunye ne-Ti-Sapphire lasers)
• Iimodyuli zesigaba, i-waveguide substrate, imigangatho yamaza acoustic angaphezulu
IiPropathi zeNdalo- LiNbO3
Ifomula yekhemikhali | LiNbO3 |
Isakhiwo sekristali | I-Trigonal |
Iqela leqela | 3m |
Iqela lesithuba | R3c |
Ii-Lattice constants | a= 5.148 Å, c= 13.863 Å, Z = 6 |
Ukuxinana | I-4.628 g / cm3 |
Indawo yokunyibilika | 1255 ° C |
Iqondo lokushisa leCurie | 1140 ° C |
Ubunzima be-Mohs | 5 |
Ukuqhutywa kweshushu | 38 W / (m · K) @ 25 ° C |
I-coefficients yokwanda kwe-Thermal | I-2.0 × 10-6/ K (// a), 2.2 × 10-6/ K (// c) |
I-Hygroscopicity | I-non-hygroscopic |
IiPropathi ze-Optical-LiNbO3
Umda weTransparent (kwinqanaba "le-0" lokudlulisa) |
400-5500 nm | ||||
Ii-indices ezihlaziyayo | 1300 nm | 1064 nm | I-632.8 nm | ||
ne= 2.146 no= 2.220 |
ne= 2.156 no= 2.232 |
ne= 2.203 no= 2.286 |
|||
I-coefficients ye-Thermal optic | dno/dT = -0.874 × 10-6/ K @ 1.4 μm dne/dT = 39.073 × 10-6/ K @ 1.4 μm |
||||
I-coarfficients emgceni |
326 nm |
1064 nm |
|||
α = 2.0 / cm | α = 0.001 ~ 0.004 / cm | ||||
Ii-NLO coefficients |
d33 = 34.4 pm / V, d22 = 3.07 pm / V, |
||||
Coefficients ze-Electro-optic | γT33= 32 pm / V, γS33= 31 pm / V, γT31= 10 pm / V, γS31= 8.6 pm / V, γT22= 6.8 pm / V, γS22= 3.4 pm / V |
||||
Ihafu-yamandla ombane (DC) | Intsimi yombane // z, ukukhanya ⊥ z | I-3.03 kV | |||
Intsimi yombane // x okanye y, ukukhanya // z | I-4.02 kV | ||||
Umqobo womqobo | 100 MW / cm2 @ 1064nm, 10 ns |